위상차 현미경법에 의한 인조광물섬유 분석 변이
Analytical Variability of Airborne Man-made Mineral Fibers by Phase Contrast Microscopy
신용철(인제대학교 보건안전공학과); 이광용(안전보건공단 산업안전보건연구원); 김부욱(근로복지공단 직업성폐질환연구소)
22권 2호, 134~139쪽
초록
Objectives:This study was conducted to study the analytical variability of A & B counting rules in counting using a phase contrast microscope airborne fibers collected on filters in man-made mineral or vitreous fibers (MMMFs) industries. Methods:Fibers in filters were counted using A & B rules of NIOSH Method 7400. Intra-counter and inter-counter variations by fiber type and density were obtained. The types of MMMFs analyzed were glass wool fiber, rock wool fiber, slag wool fiber, and refractory ceramic fibers. The densities of fibers classified were <20 fibers/㎟, 20 - <50 fibers/㎟, 50 - <100 fibers/㎟, and ≥100 fibers/㎟, respectively. Results:Intra-counter relative standard deviations by rule A were 0.084, 0.102, 0.071 for glass wool fibers, rock wool fibers and refractory ceramic fibers, and those by rule B were 0.139, 0.120 and 0.142, respectively. Inter-counter relative standard deviations by rule A were 0.281, 0.296, 0.180 for glass wool fibers, rock wool fibers and refractory ceramic fibers, and those by rule B were 0.396, 0.337 and 0.238, respectively. Conclusions:Intra-counter variation was not different significantly among fiber types (p>0.05), but B rule variation for ceramic fibers approximately 2 times greater than corresponding A rule estimates, and intra-counter and inter-counter variations were higher in the low fiber density.
Abstract
Objectives:This study was conducted to study the analytical variability of A & B counting rules in counting using a phase contrast microscope airborne fibers collected on filters in man-made mineral or vitreous fibers (MMMFs) industries. Methods:Fibers in filters were counted using A & B rules of NIOSH Method 7400. Intra-counter and inter-counter variations by fiber type and density were obtained. The types of MMMFs analyzed were glass wool fiber, rock wool fiber, slag wool fiber, and refractory ceramic fibers. The densities of fibers classified were <20 fibers/㎟, 20 - <50 fibers/㎟, 50 - <100 fibers/㎟, and ≥100 fibers/㎟, respectively. Results:Intra-counter relative standard deviations by rule A were 0.084, 0.102, 0.071 for glass wool fibers, rock wool fibers and refractory ceramic fibers, and those by rule B were 0.139, 0.120 and 0.142, respectively. Inter-counter relative standard deviations by rule A were 0.281, 0.296, 0.180 for glass wool fibers, rock wool fibers and refractory ceramic fibers, and those by rule B were 0.396, 0.337 and 0.238, respectively. Conclusions:Intra-counter variation was not different significantly among fiber types (p>0.05), but B rule variation for ceramic fibers approximately 2 times greater than corresponding A rule estimates, and intra-counter and inter-counter variations were higher in the low fiber density.
- 발행기관:
- 한국산업보건학회
- DOI:
- http://dx.doi.org/
- 분류:
- 환경/직업의학